化学成份:
碳 C :0.95~1.20
硅 Si:≤1.00
锰 Mn:≤1.25
硫 S :≤0.15
磷 P :≤0.060
铬 Cr:16.00~18.00
镍 Ni:允许含有≤0.60
钼 Mo:可加入≤0.75
Y108Cr17在交货状态下,棒材经过固溶处理,板材经过固溶酸洗。其抗拉强度为590MPa,延伸强度为245MPa,伸长率为15%,断面收缩率为一。在硬度方面,经过退火处理后,硬度为255HBW,淬火回火后硬度为58HRC。加热温度在800~920℃之间,加热方式为缓冷。